System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
HB Fuller U3349TX Structural Adhesive
Categories:
Polymer
;
Thermoplastic
;
Adhesives, Sealants, and Coatings
Material Notes:
U3349TX is a high viscosity, low/non sag, UV-curable adhesive designed for bonding a variety of plastics.
Information provided by H.B. Fuller Company
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.05
g/cc
1.05
g/cc
Viscosity
15000
-
25000
cP
15000
-
25000
cP
Storage Temperature
8.00
-
21.0
°C
46.4
-
69.8
°F
in darkness
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
70
70
ASTM D2240
Hardness, Shore D
32
32
ASTM D2240
Elongation at Break
150 %
150 %
ASTM D638
Thermal Properties
Metric
English
Comments
Flash Point
>=
95.0
°C
>=
203
°F
Processing Properties
Metric
English
Comments
Cure Time
<=
0.0833
min
<=
0.00139
hour
Set Time, at 395nm, 50mW/cm2
1440
min
24.0
hour
Full Cure Time
Shelf Life
9.00
Month
9.00
Month
Descriptive Properties
Color
Light Straw
Consistency
Liquid
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PHBFULL228 / 317019
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.