EPS has excellent physical properties, low energy consumption and has FDA compliant offerings. Its lightweight and proven performance makes it suitable for a wide variety of markets and applications including building & construction, geofoam, packaging, and cup & container. EPS enable customers to produce high-quality products that are sturdy, safe and durable. Features/Attributes: Low Density Potential, Controlled/Uniform, Expansion. Applications: Insulation, SIP's, Fabricated Packaging.Information provided by NOVA Chemicals. |