LL 3150.32 is a hexene copolymer LLDPE film resin for blown film. Films produced from this resin have excellent tensile and toughness properties, as well as improved stiffness. Combined with good drawability properties, this is a versatile packaging film resin. Information provided by ExxonMobil Chemical |