MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Panipol Oy DXH-PP Inherently Conductive Polymer
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Panipol DXH-PP composition is a conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are controllable resistance in optimal ESD protection range 10^6-10^9 Ohm, low sloughing and limited colorablity.

The conductivity of Panipol DXH-PP / matrix polymer blend is tunable from insulators into matrix polymer chain instead of acting as a filler. The conductive/dissipative property is permanent and built into the polymer chain.

Panipol DXH-PP has been developed mainly for injection molding applications. Panipol DXH-PP should be used in 10-18% ratio with PP Heterophasic copolymer to achieve surface resistance values from 10^6 to 10^10 Ohm, (IEC 61340-5-1d). The products made out of Panipol DXH-PP are resusable and recyclable.

Typical applications include injection molded boxes and bins etc. giving permanent ESD protection for the various packaging applications.

Information provided by Panipol Oy Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/cc
 
Mechanical PropertiesOriginal ValueComments
Charpy Impact, Notched 0.900 J/cm²ISO 180
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+6 - 1.00e+7 ohm
@Thickness 2.00 mm
sheet; IEC 61340-5-1
Static Decay <= 0.50 sec
@Thickness 2.00 mm
sheet; IEC 61340-5-1
 
Processing PropertiesOriginal ValueComments
Front Barrel Temperature 190 - 220 °C
Melt Temperature <= 230 °C
Mold Temperature 30.0 - 50.0 °C
Injection Pressure 10900 - 17400 psi
 
Descriptive Properties
Back PressureHigh
Injection SpeedHigh
Plasticizing SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Panipol Oy T Inherently Conductive Polymer
Panipol Oy W Dispersions Inherently Conductive Polymer
Avient Teslart™ Powder Polyaniline chains grafted to lignosulfonic acid

PPANIPOL4 / 55910

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.