MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow 722 Linear Low Density Polyethylene (LDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/closures. It complies with U.S. FDA 21 CFR 177.1520 (c) 2.1.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D792
ESCR 100% Igepal® <= 1.0 hour
@Temperature 50.0 °C
F50; Molded and tested in accordance with ASTM D4976; ASTM D1693
Melt Index of Compound 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 43Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 1400 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 1200 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 500 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 4.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 34000 psi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 130 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesOriginal ValueComments
Melting Point 224 °FDow Method (DSC)
Crystallization Temperature 95.0 °CDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 190 °FASTM D1525
Brittleness Temperature -76.0 °FMolded and tested in accordance with ASTM D4976; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 722 Low Density Polyethylene (LDPE)
Dow 959S Linear Low Density Polyethylene (LDPE)
A. Schulman CP814-01 Linear, Low-Density Polyethylene
Dow 620I Linear Low Density Polyethylene (LDPE)
Dow DMDA-8907 NT 7 High Density Polyethylene Resin

PDOW1223 / 30441

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.