MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Petro IPSA Diisopropyl Naphthalene Sulfonic Acid
Categories: Other Engineering Material

Material Notes: Anionic alkylaryl sulfonate secondary demulsifier additive for slug treaters

Applications: Witco Petro IPSA is an alky naphthalene sulfonic acid. This product may be diluted and used in the acid form, or it may be neutralized prior to dilution and use. Typically, ammonia or an inexpensive amine is utilized to neutralize Petro IPSA. Witco Petro IPSA works by effectively neutralizing the strength of the natural emulsifying agent, allowing the finely dispersed water droplets to coalesce. As the tiny water droplets merge into progressively large and heavier drops, the water settles and the oil rapidly rises to the top. The result is a sharp, well-defined oil/water interface and bright, clean and marketable oil.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.983 g/cc0.0355 lb/in³
pH <= 2.0<= 2.05% solution
Brookfield Viscosity 4500 cP4500 cP
 
Thermal PropertiesMetricEnglishComments
Pour Point -7.80 °C18.0 °F
Flash Point >= 93.3 °C>= 200 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 6.0 %<= 6.0 %
 
Descriptive Properties
AppearanceViscous Liquid, Dark Amber
OdorSolvent
Relative Solubility Number16.9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY844 / 286367

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.