Trigonox 301 is an initiator for the production of controlled rheology polypropylene (CR-PP) and high temperature polymerization of ethylene. CAS number: 24748-23-0 EINECS/ELINCS No: 429-320-2 Applications: Trigonox 301 is an efficient peroxide formulation for the production of controlled rheology polypropylene (CR-PP) in an extrusion process. An important advantage of Trigonox 301 is that the final CR-PP contains a low content of volatiles originating from peroxide decomposition products. Trigonox 301 forms no acetone and no tert-butanol. Information provided by Nouryon |