MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici RADILON® S RCW4015W 3733 BK Nylon 6, 40% Glass/Mineral Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: PA6 40% glass fiber and mineral reinforced injection molding grade, heat stabilized. Black color. Suitable for parts requiring high stiffness, good mechanical resistance and excellent heat ageing properties retention, good dimensional stability.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, Improved Dimensional Stability, High Surface Aspect

Industries: Automotive, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Viscosity Measurement 142142[ml/g]; ISO 307
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inMelt Temp/Mold Temp/Cavity Pressure: 280/90/60; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inMelt Temp/Mold Temp/Cavity Pressure: 280/90/60; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 8.80 GPa1280 ksi1mm/min; ISO 527-2/1A
Flexural Strength 190 MPa27600 psi2mm/min; ISO 178
Flexural Modulus 8.30 GPa1200 ksi2mm/min; ISO 178
Izod Impact, Notched (ISO)  5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 5.50 kJ/m²
@Temperature 23.0 °C
2.62 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.650 J/cm²
@Temperature 23.0 °C
3.09 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm500V; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohm500V; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 193 °C379 °FISO 75/2Af
Flame Spread <= 0.000 mm/min
@Thickness 3.00 mm
<= 0.000 in/min
@Thickness 0.118 in
Automotive Interior; ISO 3795
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 280 °C464 - 536 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI123 / 313624

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.