MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALCOLOR® PC A GY937-2340 Color additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: For use in: Polycarbonate

Special Features: Free from cadmium, lead and diarylide pigments, dust-free, high additive content, high dispersibility

Market Segment: Electrical and Electronic, Building and Construction, Sport and Leisure, Furniture

Application Area: Injection molded parts, extruded parts, blow molded parts

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Storage Temperature <= 30.0 °Cdry, protected from light
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °CThermal Stability Colorant
Melt Temperature 270 - 310 °CInjection molding
Mold Temperature 80.0 - 110 °CInjection molding
Drying Temperature 100 - 120 °C
@Time 7200 - 10800 sec
in a dry air (desiccant) dryer
 100 - 120 °C
@Time 14400 - 43200 sec
in air circulating dryer
 
Descriptive Properties
Base PolymerPolycarbonate
ColorGreysimilar to RAL 7035
Dosage (%)3injection molding
 3extrusion
Light Fastness Colorantblue woolscale 8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PALBIS8030 / 242089

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.