MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Texin® 260 Thermoplastic Polyurethanes (TPU) (Extended Aging Data)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Texin 260 resin is an aromatic polyester-based thermoplastic polyurethane with a Shore hardness of approximately 60D. It can be processed by injection molding; extrusion processes are not recommended.

Properties / Applications: Texin 260 resin offers outstanding abrasion resistance, impact strength, toughness, and flexibility. It also exhibits excellent fuel and oil resistance. Texin 260 natural color resin complies with FDA food-contact regulations 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber Articles Intended for Repeated Use), subject to the limitations of these and any other applicable regulations. Typical applications include toplifts, casters, grommets, and seals.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.54 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
 53
@Time 1.81e+6 sec
Fuel C; ASTM D471
 54
@Time 1.21e+6 sec
Fuel C; ASTM D471
 57
@Time 1.21e+6 sec
Fuel A; ASTM D471
 58
@Time 1.81e+6 sec
Fuel A; ASTM D471
 59
@Time 252000 sec
Fuel A; ASTM D471
 59
@Time 252000 sec
Fuel C; ASTM D471
 59
@Time 605000 sec
Fuel C; ASTM D471
 60
@Time 605000 sec
Fuel A; ASTM D471
 56
@Treatment Temp. 125 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 57
@Treatment Temp. 125 °C,
Time 605000 sec
Hot Air; ASTM D573
 57
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 57
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 57
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #3; ASTM D471
 57
@Treatment Temp. 125 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 58
@Treatment Temp. 125 °C,
Time 252000 sec
Hot Air; ASTM D573
 58
@Treatment Temp. 100 °C,
Time 605000 sec
Hot Air; ASTM D573
 58
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #1; ASTM D471
 59
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3; ASTM D471
 60
@Treatment Temp. 100 °C,
Time 252000 sec
Hot Air; ASTM D573
 60
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1; ASTM D471
 60
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #1; ASTM D471
 62
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #1; ASTM D471
Tensile Strength at Break 60.0 MPaASTM D412
 48.6 MPa
@Time 1.81e+6 sec
Fuel C; ASTM D471
 54.6 MPa
@Time 1.21e+6 sec
Fuel C; ASTM D471
 55.8 MPa
@Time 605000 sec
Fuel C; ASTM D471
 57.6 MPa
@Time 252000 sec
Fuel A; ASTM D471
 58.8 MPa
@Time 605000 sec
Fuel A; ASTM D471
 59.4 MPa
@Time 1.81e+6 sec
Fuel A; ASTM D471
 59.4 MPa
@Time 252000 sec
Fuel C; ASTM D471
 60.6 MPa
@Time 1.21e+6 sec
Fuel A; ASTM D471
 6.60 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
Hot Air; ASTM D573
 58.8 MPa
@Treatment Temp. 125 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 63.6 MPa
@Treatment Temp. 125 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 65.4 MPa
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 67.2 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1; ASTM D471
 67.8 MPa
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 67.8 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3; ASTM D471
 69.6 MPa
@Treatment Temp. 125 °C,
Time 252000 sec
Hot Air; ASTM D573
 70.2 MPa
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #1; ASTM D471
 72.0 MPa
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #1; ASTM D471
 72.6 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
Hot Air; ASTM D573
 73.2 MPa
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #1; ASTM D471
 76.8 MPa
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #3; ASTM D471
Tensile Stress 64.2 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
Hot Air; 4.2% strain; ASTM D573
Tensile Stress at Strain 20.0 MPa
@Strain 50 %
ASTM D412
 22.1 MPa
@Strain 100 %
ASTM D412
 40.0 MPa
@Strain 300 %
ASTM D412
 20.332 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 504; ASTM D573
 20.553 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 336; ASTM D573
 21.658 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 504; ASTM D471
 21.658 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 70; ASTM D573
 21.879 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 168; ASTM D471
 22.542 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 336; ASTM D471
 22.984 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 50; ASTM D471
 23.205 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 504; ASTM D471
 23.647 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 336; ASTM D471
 23.647 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 336; ASTM D471
 23.868 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 70; ASTM D471
 23.868 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 168; ASTM D573
 24.973 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 70; ASTM D471
 25.636 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 168; ASTM D471
 29.6 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 504; ASTM D573
 30.4 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 336; ASTM D573
 32.8 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 70; ASTM D573
 33.6 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 336; ASTM D471
 34.4 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 50; ASTM D471
 34.4 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 504; ASTM D471
 35.2 MPa
@Strain 300 %,
Temperature 125 °C
Hot Air, 168; ASTM D573
 38.4 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 504; ASTM D471
 38.8 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 336; ASTM D471
 39.6 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 168; ASTM D471
 40.8 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 168; ASTM D471
 42.0 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #1, 70; ASTM D471
 42.0 MPa
@Strain 300 %,
Temperature 100 °C
ASTM Oil #3, 336; ASTM D471
 43.2 MPa
@Strain 100 %,
Temperature 100 °C
Hot Air, 70; ASTM D471
 14.807 MPa
@Strain 100 %,
Time 1.81e+6 sec
Fuel C; ASTM D471
 16.796 MPa
@Strain 100 %,
Time 1.21e+6 sec
Fuel C; ASTM D471
 18.343 MPa
@Strain 100 %,
Time 605000 sec
Fuel C; ASTM D471
 18.785 MPa
@Time 252000 sec,
Strain 100 %
Fuel C; ASTM D471
 20.995 MPa
@Strain 100 %,
Time 1.81e+6 sec
Fuel A; ASTM D471
 21.216 MPa
@Time 252000 sec,
Strain 100 %
Fuel A; ASTM D471
 21.879 MPa
@Strain 100 %,
Time 605000 sec
Fuel A; ASTM D471
 22.542 MPa
@Strain 100 %,
Time 1.21e+6 sec
Fuel A; ASTM D471
 36.0 MPa
@Strain 100 %,
Time 1.81e+6 sec
Fuel C; ASTM D471
 39.6 MPa
@Time 252000 sec,
Strain 100 %
Fuel A; ASTM D471
 40.4 MPa
@Strain 100 %,
Time 1.21e+6 sec
Fuel C; ASTM D471
 40.8 MPa
@Strain 100 %,
Time 605000 sec
Fuel A; ASTM D471
 40.8 MPa
@Strain 100 %,
Time 1.21e+6 sec
Fuel A; ASTM D471
 40.8 MPa
@Strain 100 %,
Time 1.81e+6 sec
Fuel A; ASTM D471
 41.6 MPa
@Strain 100 %,
Time 605000 sec
Fuel C; ASTM D471
 44.4 MPa
@Time 252000 sec,
Strain 100 %
Fuel C; ASTM D471
Elongation at Break 420 %ASTM D412
 399 %
@Time 252000 sec
Fuel A; ASTM D471
 403.2 %
@Time 605000 sec
Fuel A; ASTM D471
 403.2 %
@Time 1.81e+6 sec
Fuel A; ASTM D471
 415.8 %
@Time 1.21e+6 sec
Fuel A; ASTM D471
 432.6 %
@Time 1.81e+6 sec
Fuel C; ASTM D471
 432.6 %
@Time 605000 sec
Fuel C; ASTM D471
 441 %
@Time 252000 sec
Fuel C; ASTM D471
 445.2 %
@Time 1.21e+6 sec
Fuel C; ASTM D471
 424.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
Hot Air; ASTM D573
 453.6 %
@Treatment Temp. 100 °C,
Time 605000 sec
Hot Air; ASTM D573
 466.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #3; ASTM D471
 466.2 %
@Treatment Temp. 100 °C,
Time 252000 sec
ASTM Oil #1; ASTM D471
 491.4 %
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
 520.8 %
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 541.8 %
@Treatment Temp. 100 °C,
Time 605000 sec
ASTM Oil #1; ASTM D471
 571.2 %
@Treatment Temp. 100 °C,
Time 1.21e+6 sec
ASTM Oil #1; ASTM D471
 604.8 %
@Treatment Temp. 125 °C,
Time 1.81e+6 sec
Hot Air; ASTM D573
 617.4 %
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #3; ASTM D471
 617.4 %
@Treatment Temp. 100 °C,
Time 1.81e+6 sec
ASTM Oil #1; ASTM D471
 634.2 %
@Treatment Temp. 125 °C,
Time 605000 sec
Hot Air; ASTM D573
 634.2 %
@Treatment Temp. 125 °C,
Time 252000 sec
Hot Air; ASTM D573
 638.4 %
@Treatment Temp. 125 °C,
Time 1.21e+6 sec
Hot Air; ASTM D573
Compressive Strength 0.340 MPa2% Deflection; ASTM D 575
 3.60 MPa5% Deflection; ASTM D 575
 9.40 MPa10% Deflection; ASTM D 575
 13.4 MPa15% Deflection; ASTM D 575
 17.4 MPa20% Deflection; ASTM D 575
 21.7 MPa25% Deflection; ASTM D 575
 53.7 MPa50% Deflection; ASTM D 575
Resilience 35[%], Bayshore; ASTM D2632
Tear Strength 175 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 50
@Load 1.00 kg
[mg] Loss, H-18; ASTM D3489
Compression Set 27 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395-B
 55 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395-B
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CASTM D648
Vicat Softening Point 190 °CRate A; ASTM D1525
Brittleness Temperature >= -68.0 °FASTM D746
Glass Transition Temp, Tg -15.0 °C
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °C
Middle Barrel Temperature 190 - 215 °C
Front Barrel Temperature 200 - 220 °C
Nozzle Temperature 205 - 225 °C
Melt Temperature 210 - 220 °C
Mold Temperature 15.0 - 40.0 °C
Injection Pressure 6000 - 15000 psi
Back Pressure <= 200 psi
Cushion <= 0.125 in
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Barlog Plastics KEBAFLEX U A 75 ST B01 natural TPU, Shore A75, natural
Covestro Texin® 245 Thermoplastic Polyurethanes (TPU)

PCOVEST0977a / 238179

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.