MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker ELASTOSIL® R 407/50 Silicone Rubber Base
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R 407/50 Silicone Rubber Bases are noted for their high transparency and good mechanical properties. Intermediate hardnesses can be achieved by blending these bases in the required proportion. Due to the high green strength of these products, they can be used to make complex extruded profiles. Their vulcanizing characteristics make it possible to achieve short cycle times in the production of rubber moldings by compression, transfer and injection molding. Post cured vulcanizates can be used for applications in the health care and food handling industries.

Special features:

  • Excellent tensile strength
  • Excellent clarity
  • Exceptional extrusion qualities
  • Excellent molding qualities

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 - 1.22 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50ASTM D746
Tensile Strength 1450 psiASTM D2240
Elongation at Break 450 %ASTM D412
Tear Strength 120 pliASTM D412
Compression Set 35 %
@Temperature 177 °C,
Time 79200 sec
WSTM 1114
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Transparent, but not quantified
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 min
@Temperature 116 °C
press cured, post cured 4 h/200 °C
 
Descriptive Properties
AppearanceTransparentWSTM 1297

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® LR 3002/35 A/B Low Viscous Liquid Rubber
Precision Polymer Engineering S50R Silicone Rubber
Precision Polymer Engineering S50A Silicone Rubber
NuSil MED-4850 Liquid Silicone Rubber - Unrestricted Medical Use
Dow Silastic® RBL-9200-50 LSR Liquid Silicone Rubber

PWACK9905 / 197504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.