MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® 349 Acrylic Light Cure Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Acrylic Light Cure Adhesives
Versatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single component, solvent-free products cure in seconds when exposed to UV/visible light sources. Some light cure adhesives can be combined with activator curing methods to meet specific application requirements.

Loctite® 349 Acrylic Light Cure Adhesive
Key Substrates: Glass, metal Cure Type: Ultraviolet, Light Bonding Type: Acrylic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 9500 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Elongation at Break 300 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
ColorClear/Straw

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 3491 Acrylic Light Cure Adhesive
Henkel Loctite® 3761 Acrylic Light Cure Adhesive
Henkel Loctite® 3751 Acrylic Light Cure Adhesive
Henkel Loctite® 3701 Acrylic Light Cure Adhesive
Henkel Loctite® 3273 Acrylic Bonding Adhesive

PLOCT060 / 51796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.