MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eneos 1300B TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Characteristics:
  • Dynamic vulcanized TPO
  • High melt flow and good injection moldability
  • Excellent adhesion with cured rubbers
  • Wide Range of hardness (20-80 (DuroA))
Typical Applications:
  • Corner moldings of weather seals
  • Various types of seals(replacement of urethane foam)

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.880 g/cc0.880 g/ccISO 1183
Melt Flow 2.0 g/10 min
@Load 2.14 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.72 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 34
@Time 15.0 sec
34
@Time 0.00417 hour
ISO 868
Tensile Strength 1.10 MPa160 psiAdhesion Test with Cured EPDM( Hs70A), 200mm/min.
 3.50 MPa508 psiISO 37(I)
Elongation at Break 110 %110 %Adhesion Test with Cured EPDM( Hs70A), 200mm/min.
 680 %680 %ISO 37(I)
100% Modulus 0.900 MPa131 psiISO 37(I)
Tear Strength 15.0 kN/m85.6 pliISO 34 B (a)
Compression Set 39 %
@Temperature 70.0 °C,
Time 79200 sec
39 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -60.0 °C<= -76.0 °F
Shrinkage 0.80 %0.80 %
 
Optical PropertiesMetricEnglishComments
Gloss 3.0 %3.0 %ISO 2813

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8141 / 295457

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.