MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond F199 High Temperature Anaerobic Adhesive System
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND F199 is a high strength, anaerobic adhesive for fiberoptic terminations. Although specifically designed for bonding glass and plastic fiber to plastic ferrules, it also bonds exceptionally well to ceramic and metal ferrules. This system gels very quickly allowing for polishing and connecting in under 2 minutes. The high temperature capability of TRA-BOND F199 allows it to be used in many non-fiber applications where a bond line under .005" is required.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccMixed
Viscosity 60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
Adhesive (sp #6, 2.5 rpm)
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 13.8 MPa2000 psiLap shear, alum to alum
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 47.0 °C117 °FUltimate Tg; TMA
 
Descriptive Properties
Color AmberPrimer
 ClearAdhesive

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC245 / 71173

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.