MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion AlBeCast™ IC910 Aluminum Beryllium Composite  (discontinued **)
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: Mechanical properties are typical values at RT. AlBeCast™ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stiffness, thermal performance, and weight savings of Al/Be materials. The casting process requires little change from Al or Ti casting.

Please note that there are health hazards associated with beryllium, especially when present as airborne particles generated during processing. As with any material, be aware of hazards and take steps to reduce exposure to a safe level.

Information provided by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 207 MPa
Tensile Strength, Yield 158 MPa
@Strain 0.2 %
Elongation at Break 4.0 %
Tensile Modulus 192 GPaDynamic modulus
 193 GPa
Compressive Yield Strength 147 MPa
Poissons Ratio 0.154
Fatigue Strength 117 MPa
@# of Cycles 1.00e+7
R=0.05; Kt = 2.16 MPa
Fracture Toughness 7.30 - 14.6 MPa-m½KQ
Shear Modulus 84.0 GPadynamic
Shear Strength 181 MPadouble pin shear (ASTM B-789)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.6 µm/m-°C
@Temperature 20.0 °C
 16.0 µm/m-°C
@Temperature 250 °C
 18.2 µm/m-°C
@Temperature 500 °C
Specific Heat Capacity 1.56 J/g-°C
Thermal Conductivity 110 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 38 %As remainder
Beryllium, Be 57 - 63 %
Iron, Fe <= 0.30 %
Nickel, Ni 2.1 - 3.4 %
Oxygen, O <= 0.24 %
Silicon, Si <= 0.50 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Materion AlBeMet® AM 162 Rolled Sheet, Annealed
Materion AlBeMet® AM 162 HIP'd Billet, Annealed
Goodfellow Aluminum-Lithium/SiC Metal Matrix Composite
Aluminum - SiC Metal Matrix Composite

NBB100 / 15089

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.