MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell A-C® 307A High-density oxidized PE homopolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Hard, high drop point, high density, higher molecular weight (MW), oxidized polyethylene (HDOxPEs) homopolymer in a finer powder form than A C 307 mainly used as a metal release agent for PVC processing. It will not affect clarity in transparent PVC applications. Its low acid number does not allow it be emulsified for use in aqueous systems, like most of Honeywells other high density oxidized polyethylene (HDOxPEs).

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³
Brookfield Viscosity 85000 cP
@Temperature 150 °C
85000 cP
@Temperature 302 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 7.07.0
 
Thermal PropertiesMetricEnglishComments
Dropping Point 140 °C284 °FMettler
 
Descriptive Properties
Hardness<0.5 dmmASTM D5
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global B-8200 High Density Polyethylene
Ipiranga Petrochem HC 7260 HDPE
IRPC Polimaxx Polene GA3245 High Density Polyethylene
Global B-6200 High Density Polyethylene
Global B-5200 High Density Polyethylene

PHONWL015 / 179560

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.