MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Network Polymers Softflex® 2910
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Softflex® Thermoplastic Elastomer Alloy

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0080 cm/cm
@Thickness 3.17 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 3.17 mm
ASTM D955
Melt Flow 0.30 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8510 second dwell; ASTM D2240
 91Instantaneous; ASTM D2240
Tensile Strength, Yield 1643 psichs 20 in/min; ASTM D412
Elongation at Break 873 %ASTM D412
50% Modulus 0.00150 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.00200 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00340 GPa
@Strain 300 %
ASTM D412
Gardner Impact 280 in-lb
@Temperature -30.0 °C
ASTM D5420
Taber Abrasion, mg/1000 Cycles 0.2409H22 Wheel 1000 g load/1000 cycles; ASTM D3389
Compression Set 95.5 %
@Temperature 70.0 °C
22 hours at 25% deflection; ASTM D395, Method B,
 97.9 %
@Temperature 100 °C
22 hours at 25% deflection; ASTM D395, Method B,
 38.5 %
@Temperature 23.0 °C,
Time 79200 sec
Method B, at 25% deflection; ASTM D395
Tensile Set 3.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Engage® 8100 Polyolefin Elastomer
Dow INFUSE™ 9530 Olefin Block Copolymer
Network Polymers Softflex® 8103
Global TPE-LS70A Elastomer Grade
Envalior Arnitel® EL250 TPC-ET, Injection Molding

PDIAM011 / 29849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.