MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wacker Silres® BS 1801 Concrete Admixture
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® BS 1801 is a mixture of octyltriethoxysilanes isomers, with iso-octyltriethoxysilane as the main component. SILRES® BS 1801 is used in undiluted form as an admixture for the integral waterproofing of fresh concrete.

Special features: In the fresh concrete SILRES® BS 1801 reacts with the water in the building material’s pores, eliminating alcohol. The active thus substance formed greatly reduces the concrete’s absorbency, but without blocking any pores or capillaries. The impregnated building material retains very high water-vapor permeability.

Application: SILRES® BS 1801 is recommended as a waterproofing concrete admixture.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.880 g/ccDIN 51757
Viscosity 1.9 cPdynamic; DIN 51562
Molecular Weight 276 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 236 °C
@Pressure 0.1013 MPa
Flash Point >= 40.0 °CISO 3679
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear colorless
Content (%)99Silane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9554 / 205083

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.