MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SHRINK® Tubing Conductive Heat Shrinkable EMI Shielding
Categories: Polymer; Thermoset

Material Notes: Description: CHO-SHRINK tubing is a heat shrinkable polyolefin manufactured to MIL-R-46846 Type 5, modified to provide effective 360° EMI shielding for cables. CHO-SHRINK tubing offers significant weight savings over conventional metal braid shielding, and can be applied easily with standard shrink tubing heating devices. The main feature of CHO-SHRINK tubing is Chomerics’ unique conductive coating. Which is applied to the surface of the tubing and which remains flexible, uniform and intact even after maximum shrinking. The coating, a silver-based system, can be applied to the inside or outside surfaces, or both. Standard CHO-SHRINK products may be recovered (shrunk) with the same heating equipment used on ordinary nonconductive shrinkable plastics.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1500 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 19.7 kV/mmASTM D876
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -54.0 °C
 
Descriptive Properties
DC Resistance1 ohm/ft
Shrink Ratio2:1
Shrink Temperature121 - 191°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch® FP-301 Heat Shrink Tubing
3M MW Heat Shrink Tubing
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
Kolon CS101 Heat shrinkable PET Film
3M EPS-400 Heat Shrink Tubing

PCHOME240 / 130950

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.