MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Koattro KT MR 05 Plastomer
Categories: Polymer; Film; Thermoplastic

Material Notes: Koattro is a novel family of high-molecular-weight plastomers. Koattro KT MR05 is a plastomeric material based on LyondellBasell technology and is highly compatible with Polypropylene (PP). This product blended with PP enhances softness, elastic recovery, elongation at break and impact resistance whilst improving transparency and reducing stress whitening. Koattro KT MR05 is available in free flowing pellet form. Applications: Appliances, Automotive Parts, Coatings, Protective, Color Concentrates, Industrial, Polymer Modifier, Products for Use in Property Modification, Sealants, Surface Protection Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.870 g/cc0.0314 lb/in³ISO 1183-1
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ISO 868
Tensile Strength at Break 12.0 MPa1740 psispecimens conditioned for 10 days at 23°C; ISO 8986-2
Elongation at Break >= 800 %>= 800 %specimens conditioned for 10 days at 23°C; ISO 8986-2
Flexural Modulus <= 0.0100 GPa<= 1.45 ksispecimens conditioned for 10 days at 23°C; ISO 178
Charpy Impact, Notched NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
ISO 179
Compression Set 30 %
@Temperature 23.0 °C
30 %
@Temperature 73.4 °F
25% deformation; ASTM D395
 
Descriptive Properties
Processing MethodBlown Film, Calendaring, Cast Film, Compression Molding, Continuous Filament/Spinning, Injection Molding, Spunbond

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQT7597 / 219234

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.