MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramacast™ 905 Silicone-Ceramic Potting Compound
Categories: Ceramic; Oxide; Silicon Oxide; Polymer; Thermoset; Silicone

Material Notes: Ceramacast™ 905 is a silicone-bonded, ceramic filled high temperature adhesive and potting compound. Two-component (liquid + powder), Moisture Resistant Silicone, Coarse Grain Compound.

Cure:
Step 1. Dry for 24 hours room temperature to allow solvent to evaporate.
Step 2. Bake at 150 ºF for 1 hour.
Step 3. Bake at 250 ºF for 1 hour.
Step 4. Bake at 350 ºF for 1 hour.
Step 5. Final cure at 450 ºF for 1 hour.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.575 g/cc0.0208 lb/in³Liquid
 1.15 g/cc0.0416 lb/in³Powder
Porosity <= 0.50 %<= 0.50 %after 900°F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm
Dielectric Strength >= 9.84 kV/mm>= 250 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.60 µm/m-°C2.00 µin/in-°F
Maximum Service Temperature, Air 482 °C900 °F
Shrinkage <= 1.0 %
@Temperature 482 °C
<= 1.0 %
@Temperature 900 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 65.6 - 232 °C
0.500 hour
@Temperature 150 - 450 °F
 720 - 960 min
@Temperature 22.0 °C
12.0 - 16.0 hour
@Temperature 71.6 °F
Shelf Life 6.00 Month6.00 MonthLiquid
 12.0 Month12.0 MonthPowder
 
Descriptive Properties
Acid ResistanceGood
Alkali ResistanceGood
BinderSilicone
ColorOff-White
Mix Ratio by Weight2:1powder:liquid
Moisture ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron™ D7000 PI Unfilled Polyimide
Carlisle 201LL Carbon-Carbon Composite
Kraton® FG1901 + PA-6 blend (20/80)
Mitsubishi Chemical Advanced Materials Duratron™ CU60 PBI Polybenzimidazole, unfilled, compression molded
NRI Syntho-Steel™

PAREM41a / 138302

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.