MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODAFAC® LO-11/ALA Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Phosphate ester designed for use in diesel and crude oils, where it will react with specific organometalic complexors to form very high viscosity crosslinked oil gels.

Chemical Name: ALKYL PHOSPHATE ESTER

CAS: 68412-60-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODACAL® LO-11/ALA is a phosphate ester designed for use in diesel and crude oils, where it will react with specific organometalic complexors to form very high viscosity corsslinked oil and gas wells which may be sensitive to contact with aqueous fluids or where extremely low surface temperatures make use of aqueous fluids impractical. Slow rise in “pH” from formation water or added ingredient breaks gel.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 2.0IPA/Water sol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 188 - 198pH 5-5.5; RP-0432
 200 - 215pH 9-9.5; RP-0432
 
Thermal PropertiesOriginal ValueComments
Pour Point <= -20.0 °CRP-0461
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 2.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClean, Clear to Slightly Hazy LiquidRP-0064
CompositionActivity<95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Skydrol® LD4 Fire Resistant Hydraulic Fluid
Eastman Skydrol® 500B-4 Fire Resistant Hydraulic Fluid

WRHOD355 / 137586

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.