MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® H74F Thermally Conductive, Electrically Insulating Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Material Description: A two component, high Tg, thermally conductive, electrically insulating epoxy designed for semiconductor packaging including heat sinking, hermetic sealing, and opto-electronic assemblies. It may be used for flip chip underfill, sealing sensor devices packaged in TO-cans or fiber optic feed-through. It may be considered a finer particle version of EPO-TEK® H74.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccPart B
 2.02 g/ccPart A
Particle Size <= 20 µm
Viscosity 45000 - 75000 cP
@Temperature 23.0 °C
5 rpm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 20 ppm
Ionic Impurities - K (Potassium) 9.0 ppm
Ionic Impurities - Cl (Chloride) 41 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88
Tensile Modulus 638000 psiStorage
Shear Strength >= 2000 psiLap
 >= 5100 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 5.00e+13 ohm-cm
Dielectric Constant 4.9
@Frequency 1000 Hz
Dissipation Factor 0.012
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µm/m-°CBelow Tg
 108 µm/m-°CAbove Tg
Thermal Conductivity 0.520 W/m-K
Maximum Service Temperature, Air 250 °CContinuous
 350 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 90.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 486 °CDegradation Temperature
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 150 °C
Minimum
 10.0 min
@Temperature 120 °C
Minimum
 20.0 min
@Temperature 100 °C
Minimum
Pot Life 180 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorAmberPart B
 Dark GrayPart A
ConsistencySmooth paste
Ionic Impurities NH4100 ppm
Mix Ratio by Weight100:4
Number of ComponentsTwo
Thixotropic Index1.9
Weight Loss0.05%200°C
 0.05%250°C
 0.1%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61LV Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H63 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® T905-1 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H61ND Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H70E-TI Thermally Conductive, Electrically Insulating Epoxy

PPOXYT082 / 141121

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.