MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® MonoPlus MP 800 OH Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus MP 800 OH is a strongly basic, macroporous anion exchange resin (type I) with beads of uniform size (monodisperse) based on a styrene-divinylbenzene copolymer, in highly regenerated form, designed for all polishing applications. The monodisperse beads have chemical and osmotic stability. The extremely high monodispersity (uniformity coefficient: max 1.1) and very low fines content of max. 0.1% ( <0.315 mm) result in particularly low pressure losses compared with standard resins. Lewatit MonoPlus MP 800 OH stands for effective adsorption and desorption of naturally occurring organic substances. Lewatit MonoPlus MP 800 OH is especially suitable for:
  • polishing using the Lewatit Multistep System or a conventional mixed bed arrangement in combination with Lewatit MonoPlus SP 112 H or Lewatit MonoPlus S 108 H
  • condensate polishing in combination with the Lewatit MonoPlus SP 112 H or Lewatit MonoPlus S 200 KR
  • demineralization of water for industrial steam generation operated with co-current or modern counter-current systems like e.g. Lewatit WS System, Lewatit Liftbed System or Lewatit Rinsebed SystemLewatit MonoPlus MP 800 OH adds special features to the resin bed:
    • High flow rates during regeneration and loading
    • a good utilization of the total capacity
    • a low demand for rinse water
    • a homogeneous throughput of regenerants, water and solutions, resulting in a homogeneous operating zone
    • a virtually linear pressure drop gradient across the entire bed depth, allowing operation with higher bed depths
    • a good separation of the components in mixed bed applications

    Information provided by Lanxess.

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Bulk Density 0.650 g/cc0.0235 lb/in³
    Density 1.05 g/cc0.0379 lb/in³
    Bead Size 0.600 - 0.700 mm0.0236 - 0.0276 inMean
    Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
     
    Thermal PropertiesMetricEnglishComments
    Maximum Service Temperature, Air 70.0 °C158 °F
     
    Processing PropertiesMetricEnglishComments
    Shelf Life 12.0 Month12.0 Month
     
    Descriptive Properties
    AppearanceBeige, opaque
    pH Operating Range0 - 12

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Lanxess LEWATIT® MonoPlus S 215 KR Cation Exchange Resin

    PLANY8793 / 209185

    Master Bond adhesives

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.