MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay Sulfuric Acid 98% Water White Grade
Categories: Fluid

Material Notes: Description Water White Sulfuric Acid is a clear, colorless oily-looking liquid. It is very corrosive.

Formula: H2SO4 (in aqueous solution)

Nomenclature: Sulfuric Acid, Oil of Vitriol

CAS: 7664-93-9

CAS Index: Sulfuric Acid

Available in: North America

Uses: Applications where a clear product is important in Agricultural, Chemical, Metals, Petroleum, Textiles, Water Treatment and other processes.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 98.1 g/mol
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Fe (Iron) <= 50 ppm
 
Descriptive Properties
Assay98.5-99.7%
Color<30APHA
 <30Hazen
CompositionNitrates<100 ppm
 Oxidizable organics<5 ppm
 Sulfurous Acid<50 ppm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Sulfuric Acid 98% Technical Grade

WRHOD320 / 137551

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.