MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced

Material Notes:
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage 0.0090 - 0.014 cm/cm
@Thickness 3.20 mm
72 hr; ASTM D955
 0.011 - 0.016 cm/cm
@Thickness 3.20 mm
48 hr, at 121°C; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6415 sec delay; ASTM D2240
Tensile Strength, Ultimate 38.0 MPaat max load; ASTM D638
 40.0 MPa20 in/min, at max load; ASTM D412
Elongation at Break 430 %20 in/min; ASTM D412
Flexural Modulus 0.234 GPa1.3 mm/min; ASTM D790
Tear Strength 1180 pli2 in/min; ASTM D624
Compression Set 24 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; ASTM D395
 25 %
@Temperature 23.0 °C,
Time 79200 sec
Method B; ASTM D395
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM E831
 
Descriptive Properties
Heat Sag 8 mmASTM D3769, at 121°C, 6 in. over hang

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
BASF Elastollan® R 3001 15% Glass Filled TPUR
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
A. Schulman POLYPUR™ FPU 1117 Thermoplastic Polyurethane Compound
AISI M1008 Merchant Quality Carbon Steel, Composition Spec

PASHU267 / 25231

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.