Georgia Gulf CL-7049 is a clear, high impact vinyl compound formulated for medical and food contact uses. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |