System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
NAECO® NAECOMET® 3000 AMS-T-21014 AMS-7725 High Density Machinable Tungsten
Categories:
Metal
;
Nonferrous Metal
;
Refractory Metal
;
Tungsten Alloy
Material Notes:
Uses: Radiation Shielding, High Mass, Gyro, Ordnance. Machinability is similar to gray iron.
Information provided by NAECO, LLC.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
17.24
g/cc
0.6228
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell A
63
@Temperature 600 °C
63
@Temperature 1110 °F
32 HRA
Hardness, Rockwell C
25
25
Tensile Strength, Ultimate
862
MPa
125000
psi
Tensile Strength, Yield
607
MPa
88000
psi
Elongation at Break
18 %
18 %
Modulus of Elasticity
352
GPa
51100
ksi
Compressive Yield Strength
603
MPa
87500
psi
Fatigue Strength
427
MPa
61900
psi
High cycle unnotched
427
MPa
61900
psi
High cycle unnotched
Charpy Impact
9.50
J
7.01
ft-lb
Notched
Charpy Impact, Unnotched
203
J
150
ft-lb
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.00001724
ohm-cm
0.00001724
ohm-cm
Thermal Properties
Metric
English
Comments
CTE, linear
4.61
µm/m-°C
@Temperature 20.0 - 400 °C
2.56
µin/in-°F
@Temperature 68.0 - 752 °F
5.36
µm/m-°C
@Temperature 20.0 - 800 °C
2.98
µin/in-°F
@Temperature 68.0 - 1470 °F
Thermal Conductivity
75.7
W/m-K
525
BTU-in/hr-ft²-°F
Melting Point
1425
-
3410
°C
2597
-
6170
°F
Solidus
1425
°C
2597
°F
Liquidus
3410
°C
6170
°F
Component Elements Properties
Metric
English
Comments
Copper, Cu
3.0 %
3.0 %
Nickel, Ni
7.0 %
7.0 %
Tungsten, W
90 %
90 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Kennametal Densalloy™ DENS23
MarkeTech 90-7-3 Tungsten Alloy, AMS-T-21014 Class 1
NAECO® NAECOMET® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten
ASTM A897/A897M-06 Grade 1 (130-90-09) Austempered Ductile Iron
Kennametal Densalloy™ SD175
NCMV805 / 192356
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.