System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC XENOY™ X2420 PC+PBT (Asia)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Material Notes:
XENOYX2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad color space.
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.28
g/cc
ASTM D792
Density
1.28
g/cc
ISO 1183
Water Absorption
0.020 %
23°C/sat; ISO 62
Moisture Absorption
0.0400 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0015
-
0.0025
cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse
0.0030
-
0.0040
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
26
g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
35.0
MPa
5 mm/min; ASTM D638
37.0
MPa
5 mm/min; ISO 527
Tensile Strength, Yield
50.0
MPa
5 mm/min; ASTM D638
51.0
MPa
5 mm/min; ISO 527
Elongation at Break
7.0 %
5 mm/min; ISO 527
Elongation at Yield
3.0 %
5 mm/min; ISO 527
3.0 %
5 mm/min; ASTM D638
Tensile Modulus
3800
MPa
5 mm/min; ASTM D638
Flexural Yield Strength
90.0
MPa
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
3500
MPa
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched
205
J/m
ASTM D256
Izod Impact, Unnotched
1600
J/m
ASTM D4812
Izod Impact, Notched (ISO)
14.0
kJ/m²
80*10*4; ISO 180/1A
8.00
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
110
kJ/m²
80*10*4; ISO 180/1U
74.0
kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched
95.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
95.0
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
15.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
7.00
kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
36.0
J
ASTM D3763
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
40.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
50.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow
80.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
90.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
111
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
101
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
118
°C
Rate B/120; ISO 306
UL RTI, Electrical
75.0
°C
UL 746B
UL RTI, Mechanical with Impact
75.0
°C
UL 746B
UL RTI, Mechanical without Impact
75.0
°C
UL 746B
Flammability, UL94
HB
@Thickness 0.400 mm
UL 94
Processing Properties
Original Value
Comments
Processing Temperature
60.0
-
80.0
°C
Hopper Temperature
Nozzle Temperature
260
-
290
°C
Injection Molding
Zone 1
250
-
280
°C
Zone 2
255
-
290
°C
Zone 3
255
-
290
°C
Melt Temperature
260
-
290
°C
Mold Temperature
60.0
-
90.0
°C
Drying Temperature
95.0
-
105
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
8.00
hour
Cumulative; Injection Molding
Moisture Content
0.020 %
Back Pressure
0.300
-
0.700
MPa
Shot Size
30 - 80 %
Vent Depth
0.00380
-
0.00760
cm
Screw Speed
40
-
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10846 / 244313
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.