MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Decahydronaphthalene Specialty Solvent
Categories: Fluid; Solvent

Material Notes: Decahydronaphthalene is a cyclo-aliphatic hydrocarbon with characteristic odor. It is insoluble in water but miscible with organic solvents. The mixture of isomers contain approximately 60% trans-Decahydronaphthalene.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.870 - 0.895 g/ccDIN 51 757/ ASTM D 2111
Viscosity 2.1 cPtrans isomer; DIN 53 015
 3.4 cPcis isomer; DIN 53 015
Molecular Weight 138.3 g/mol
Vapor Pressure 0.00100 bar
@Temperature 50.0 °C
cis isomer
 0.00400 bar
@Temperature 50.0 °C
trans isomer
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 279.1 J/gtrans isomer
 287.8 J/gcis isomer
Melting Point -43.0 °Ccis isomer; DIN ISO 3016
 -30.0 °Ctrans isomer; DIN ISO 3016
Boiling Point 185 - 195 °C
@Pressure 0.1013 MPa
DIN 53 171
Flash Point 54.0 °CDIN EN 22 719 / ISO 2719
 61.0 °CDIN EN 22 719 / ISO 2719
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.472n25d; DIN 51 423
 
Descriptive Properties
Evaporation Number100DIN 53 170; cis isomer
 100DIN 53 170; trans isomer
Solubility parameter at 25°C ((J/cm3)1/2)17trans isomer
 17.6cis isomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHUMB345 / 81347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.