MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil HD 50330 High Density Polyethylene Copolymer Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: ExxonMobil™ HD 50330 is a narrow molecular weight hexene copolymer designed to maximize injection molding speed and productivity in thinwall articles.Lower processing temperatures enable production of products free of taste and odor for food and beverage packaging

Availability: Latin America, North America

Additive:

  • Antioxidant: Yes
Applications:
  • Food Packaging Containers
  • Food Service Trays
  • Houseware Articles
  • Housewares
  • Toys

Information provided by ExxonMobil

Key Words: HDPE HD 6733.17
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccExxonMobil method
ESCR 10% Igepal® <= 1.00 hourF50; ASTM D1693B
Melt Flow 33 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3400 psiASTM D638
Elongation at Break 20.0 %ASTM D638
Flexural Modulus 140000 psi
@Strain 2 %
Secant; ASTM D790B
Flexural Modulus, 1% Secant 170000 psiASTM D790B
Izod Impact, Notched 0.420 ft-lb/in
@Temperature -40.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 265 °FPeak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 161 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °FASTM D648B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Escorene® HD-6733 HDPE, Injection Grade
ExxonMobil HD 6719.17 High Density Polyethylene Copolymer Resin
ExxonMobil Escorene® HD-6705 HDPE, Injection Grade
Dow DMDA-8920 NT 7 High Density Polyethylene Resin
ExxonMobil HD 6719.62 Injection Molding Resin

PEX99302 / 175538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.