MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond Ablebond 724-1 Polyurethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: Ablebond 724-1 premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc
@Temperature 23.9 °C
1.10 g/cc
@Temperature 75.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8686
Tensile Strength, Yield 31.7 MPa4600 psi
Elongation at Yield 450 %450 %
Compressive Strength 0.0621 MPa9.00 psiMethod A, 22 hrs @ 158°F under 1350 psi
 0.179 MPa26.0 psiMethod B, 22 hrs @ 158°F
Adhesive Bond Strength 13.8 MPa2000 psiLap shear, alum to alum
Tear Strength 12.3 kN/m70.0 pliSplit
Graves Tear Strength 96.4 kN/m550 pli
Abrasion 175175Abrasion Index (Bureau of Standards)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  95.0 µm/m-°C
@Temperature 23.9 - 100 °C
52.8 µin/in-°F
@Temperature 75.0 - 212 °F
 143 µm/m-°C
@Temperature 0.000 - 23.9 °C
79.4 µin/in-°F
@Temperature 32.0 - 75.0 °F
Thermal Conductivity 1.59 W/m-K11.0 BTU-in/hr-ft²-°F
Shrinkage 1.0 %1.0 %Linear
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min
@Temperature 73.9 °C
3.00 hour
@Temperature 165 °F
Pot Life 60 min60 min
Shelf Life 2.00 Month
@Temperature -40.0 °C
2.00 Month
@Temperature -40.0 °F
 
Descriptive Properties
Color Clear, Amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 724-20 Polyurethane Adhesive
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive
Tra-Con Tra-Bond FS501 Thermally Conductive Electrically Insulating Compound

PTRAC142 / 71070

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.