Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 44% Filler by Weight Additive: Lubricant and Heat Stabilizer Features: Lubricated and Heat Stabilized TPCI# 9571102 Information provided by TP Composites, Inc. |