MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Struktol VCS 526A Co-Stabilizing Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Blend fatty acid derived and functional inorganic materials.

Applications: STRUKTOL® VCS-526A is recommended for us with recycled rigid PVC where additional stabilization and lubrication is needed to reduce yellowing, burning and sticking in extrusion, injection molding and calendering. It is especially useful in allowing higher loadings of PVC regrind (post industrial or post consumer) in virgin formulations. It also allows for longer production runs between shutdowns due to degradation.

Information provided by Struktol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.113 g/cc
Additive Loading 0.50 - 2.0 %
Ash 29 - 35 %
 
Thermal PropertiesOriginal ValueComments
Dropping Point 142 - 147 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 24.0 Month
 
Descriptive Properties
AppearanceWhite to pale yellow pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTRUK47 / 69274

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.