MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Marco Polo MarPol LDC 780 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: MARPOL® LDC 780 low-density polyethylene is a general-purpose formulation used for extrusion coating and laminating. It can be drawn down to low coating weights, is processable at high speeds, has good moisture barrier, and is heat-sealable at low temperatures. MARPOL® LDC 780 can also be used for injection molding of caps and closures (flip top and gable top caps).

Recommended application: Medium and lightweight coatings and laminations, substrate coatings to provide heat sealability, hot melt adhesive, general purpose coatings, and injection molding of caps and closures.

Additives: Antiblock - no, slip - no.

Processing: MARPOL® LDC 780 has very good flow properties which allow high speed coatings at weights from 4lbs/3000sq. ft. and up. Melt temperatures of 575°F- 625°F (302°C – 330°C) are suggested.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D1505
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 10.0 MPa1450 psiASTM D638
Elongation at Break 400 %400 %ASTM D638
Tensile Modulus 0.138 GPa20.0 ksiASTM D1709
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °FASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO086 / 283683

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.