MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Huntsman Iroprint™ F 80213 TPU Protoyping Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: IROPRINT F 80213 is a polyether-based Thermoplastic Polyurethane (TPU) for Fused Filament Fabrication (FFF). Key features are high elasticity, abrasion resistance, cut and scratch resistance and good low temperature performance. It offers a good hydrolysis resistance. IROPRINT F 80213 delivers prints with a mat finish, resulting in a high-quality touch and feel of the final object.

Applications: Footwear, hoses and gaskets, robotic grippers, seals and other applications that need to be soft and elastic, yet strong and tough.

Information provided by Huntsman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.004 g/cc0.03627 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85
@Time 3.00 sec
85
@Time 0.000833 hour
ISO 7619
Hardness, Shore D 35
@Time 3.00 sec
35
@Time 0.000833 hour
ISO 7619
Tensile Strength 10.0 MPa1450 psiZ Orientation; DIN 53504
 29.0 MPa4210 psiXY Orientation; DIN 53504
Elongation at Break 320 %320 %Z Orientation; DIN 53504
 590 %590 %XY Orientation; DIN 53504
Tear Strength 26.0 kN/m148 pliZ Orientation; ISO 34-1
 90.0 kN/m514 pliXY Orientation; ISO 34-1
Abrasion 8282mm3; XY Orientation; ISO 4649
Compression Set 24 %
@Temperature 23.0 °C,
Time 252000 sec
24 %
@Temperature 73.4 °F,
Time 70.0 hour
XY Orientation; ASTM D395
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 °C473 °F
 
Descriptive Properties
Bed Temperature20-80°C
Extrusion Multiplier (Flow)1.8
Fan Speed100%
Nozzle Diameter0.4 mm
Print Speed10-100 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHU9882 / 255830

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.