MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Esenttia 60C90ND Impact Block Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Characteristics: High melt flow rate control reologhy Impact block copolymer polypropylene; good impact/stiffness balance; tough weld line; with nucleant and mold release additives.

Recommended for: Injection molding of thin wall rigid containers, fast cycle time; injection molding general purpose applications.

Information provided by Esenttia by Propilco

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238B
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 24.82 MPa50 mm/min; ASTM D638
Elongation at Yield 5.2 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1206.6 MPa1.3 mm/min; ASTM D790-1A
Izod Impact, Notched 58.72 J/mASTM D256-A
Gardner Impact 12.43 J
@Temperature 23.0 °C
ASTM D5420A
 22.6 J
@Temperature -30.0 °C
ASTM D5420A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 4624WZ Polypropylene, Impact Copolymer
Total PPC 4280W Polypropylene, Impact Copolymer
Global PP-2300-NC Polypropylene Block Copolymer
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection

PESEN053 / 184625

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.