PETROTHENE LP540200 is a copolymer resin designed for blown film applications. This resin offers high ESCR, stiffness, excellent appearance and bubble stability. LP540200 is recommended for high strength multi-wall sack liners and barrier sheeting. It is also useful as a blend component for improved stiffness and machinability. Regulatory Status: LP540200 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. This product is from the former Equistar product line. |