MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ICO Polymers ICOTEX™ 520-5076 500 Micron EVA Powder
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Description: ICOTEX 520-5076 is an EVA powder that has been developed to meet the special requirements of the textile coating industry. Its key characteristics are a good melt flow and flexibility, and a vinyl acetate content of 20%.
Key Characteristics: high toughness, good melt and strength.

Information provided by ICO Polymers.

A Schulman acquired ICO, Inc. in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D1505
Particle Size >= 150 µmpan, 7%
 <= 500 µmsieve < 5%
Vinyl Acetate Content 20 %wt %; Exxon Mobil
Melt Index of Compound 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6.00 MPaASTM D638
Elongation at Break 240 %50 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 83.0 °CDSC; ASTM D3418
 90.0 °Cfusing temperature
Vicat Softening Point 49.0 °CASTM D1525
 
Descriptive Properties
Max Dry Flowmax 37 sec/100gASTM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ICO Polymers ICOFLO™ 510-5003 1000 Micron EVA Powder
LyondellBasell Plexar® PX1164 Extrudable Tie-Layer Resin - Anhydride Modified EVA
Honeywell A-C® 400A EVA copolymer
Honeywell A-C® 405T EVA copolymer
Honeywell A-C® 405S EVA copolymer

PICO041 / 48014

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.