MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Stanelco Bioplast® GS 2189 Biodegradable Plastic
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic

Material Notes: Bioplast 2189 is a product that is optimised for sheet extrusion, injection and compression moulding. It is always biodegradable and readily compostable in thin sections, this material is useable in existing moulds and equipment and can be coloured vividly.

Bioplast 2189 is a natural replacement for PVC, PP, HDPE and PET. It is a bio-compostable material made from over 60% sustainable crop material and 20% non oil-based products.

Made from corn starch mixed with other proprietary brand products for superior flexibility, Bioplast 2189 polymer is certified EN 13432 and DIN CERTCO biodegradable and compostable. Bioplast 2189 has EU & FDA (USA) Food Contact Approval.

Bioplast 2189 was developed for the packaging, consumer and industrial sectors. Applications include formed parts and film usage, i.e. trays, pouches, wrapping, parts, lids, cups and containers. The product is versatile and can be made into sheet for thermoforming, blown into thin sheet for film, or injection moulded into virtually any shape. Bioplast 2189 has the ability to ‘drop into’ most applications with little adjustment or affect on performance.

Information provided by Stanelco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.880 - 0.940 g/ccDIN 53466
Density 1.20 - 1.40 g/ccDIN 53479/A
Melt Density 1.10 - 1.30 g/ccDIN 53735
Particle Size 2000 - 3000 µmDiameter per caliper rule
Oxygen Transmission Rate 40.0 - 60.0 cc/m²/day400 µm; ASTM F1927-98
Carbon Dioxide Transmission 60.0 - 80.0 cc-mm/m²-24hr-atm400µm; ASTM D1434
Thickness >= 10.0 micronsDIN 53353
Melt Flow 15 - 40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
DIN 53735
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 10 - 30 %DIN 53455
Film Elongation at Break, TD 10 - 30 %DIN 53455
Film Tensile Strength at Break, MD 30.0 - 45.0 MPa50% RH; DIN 53455
Film Tensile Strength at Break, TD 30.0 - 45.0 MPa50% RH; DIN 53455
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %BIOTEC Test
Shelf Life 6.00 Monthwith proper storage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FKuR Kunststoff Biograde® C 9550 Biodegradable Plastic Compound
Stanelco Bioplast® GF 106 Biodegradable Plastic
Wacker Vinnapas® EP 1400 Vinyl Acetate Ethylene
Wacker Vinnex® 2525 Vinyl Acetate Homopolymer
Bamberger Polymers Bapolene® 3252 Polyethylene, Injection Grade

PSTAN02 / 79738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.