MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Persian Gulf Polymer LLDPE-LL22B03AA
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: 22B03 is a LLDPE blown film grade designed for applications requiring good optical properties even at low extrusion temperature. This resin combines ease of processing with low gels and it is well suited for blending with LDPE and for general purpose applications. Application: High stiffness Blown film, Blending, Lamination. Features: High stiffness Blown film, Blending, Lamination. Additives: Antioxidant.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 - 0.924 g/cc0.0332 - 0.0334 lb/in³ASTM D1505
Melt Flow 2.8 - 3.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.8 - 3.2 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 50.0 MPa7250 psiASTM D882
Film Tensile Strength at Yield, TD 24.0 MPa3480 psiASTM D882
Film Elongation at Break, MD 480 %480 %ASTM D882
Film Elongation at Break, TD 850 %850 %ASTM D882
Tensile Modulus 0.115 GPa16.7 ksiMD; ASTM D882
 0.120 GPa17.4 ksiTD; ASTM D882
Elmendorf Tear Strength MD 90 g90 gASTM D1922
Elmendorf Tear Strength TD 350 g350 gASTM D1922
Dart Drop Test 70.0 g0.154 lbASTM D1709
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Gloss 90 %90 %45°; ASTM D2457
Yellow Index 0.50 %0.50 %ASTM D1925
 
Descriptive Properties
F/E Ratio<30ASTM D1238. Ratio of MIF (190 °C/2.16 Kg) / MIE (190°C/2.16Kg)
Fish Eye Note60-100 Gels/m2MTM 17108
Titanium Content (%)2Pgm wt; MTM 15636

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI975 / 250379

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.