Processed by selective laser sintering (SLS). Windform® XT 2.0 is the evolution of the ground breaking high performance Windform® XT, the carbon fiber reinforced composite material, known for its mechanical properties, which made it particularly suitable in demanding applications such as motorsport sector, aerospace and UAV’s. Windform® XT 2.0 is an innovative material, and replaces the Windform® XT, as the “Top Level” of the current Windform® range. Windform® XT 2.0 improves mechanical properties compared to “traditional” Windform® XT, while maintaining the same workability for Laser Sintering machines in order to better fulfill the needs of Additive Manufacturing required to produce end use parts and prototypes. Windform® XT 2.0 retains the matte black colour of the previous version and features improvements in mechanical properties: +8% in tensile strength, +22% in tensile modulus and +46% increase in elongation at break. Windform XT® 2.0allows for the creation of accurate, reliable and durable prototypes and is perfect for functional applications. Sample applications: Windform® XT 2.0 is the high-tech material for Additive Manufacturing chosen by those working in the Motorsport, Automotive (suitable for example for components under the hood, such as intake manifolds and functional cooling ducts), Air (for components UAV, Unmanned Aerial Vehicle) Aerospace (useful also to create prototype satellite, such as the CubeSat) and Design, as it allows applications that are fully functional, as well as bench testing, or testing and racing on the track. Information provided by CRP Technology. |
About CRP Technology CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |