MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Applications:
  • Interior trim
  • IP structural components
  • Scuff/kick plates

Injection molding conditions reported in table.

Information provided by RheTech Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
@Temperature 23.0 °C
23/23°C; ASTM D792
Filler Content 15 %ASTM D5630
Linear Mold Shrinkage 0.0105 cm/cmASTM D955
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength at Break 3000 psi2 in/min; ASTM D638
Flexural Modulus 200000 psiTangent; ASTM D790
Izod Impact, Notched 1.70 ft-lb/in
@Temperature 23.0 °C
ASTM D256
Gardner Impact 16.7 ft-lbASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 214 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 380 - 430 °F
Middle Barrel Temperature 390 - 440 °F
Front Barrel Temperature 400 - 450 °F
Nozzle Temperature 410 - 430 °F
Mold Temperature 80.0 - 120 °F
Drying Temperature 150 - 180 °F
Dry Time 1 - 2 hour
Moisture Content <= 0.050 %Recommended
Injection Pressure 400 - 1500 psi
Hold Pressure 300 - 1200 psi
Back Pressure 50.0 - 150 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Thermylene® P-20TC-0736 20% Talc Filled, Heat Stabilized Polypropylene
LyondellBasell Hostacom™ GP622 Polypropylene Homopolymer
RTP Company RTP 128 HF  Polypropylene (PP) Talc 20% - High Flow
RTP Company RTP 128 HI FR  Polypropylene (PP) Talc 20% - High Impact - Flame Retardant
RTP Company RTP 128 HI Polypropylene (PP), High Impact - Talc

PRHET239 / 65807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.