Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in laminated structures. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Outstanding optical properties
- Good seal strength
- Good dimensional stability
- Good hot slip
- Good hot tack
Features:- In Lamination Lap Sealable
Applications:- Bakery
- Biscuits/Cookie/Crackers
- Box Overwrap
- Confectionery, Chocolate
- Confectionery, Gum
- Confectionery, Sugar
- Crisps and Snacks
- Fresh Produce
- Frozen Food
- Health and Beauty Care
- Household and Detergents
- Ice Cream
- Paper Ream wrap
- Pet Food
Uses: - HFFS Flexible Packaging
- Pre-made Bags – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil |