MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips K-Resin® KR03BR SBC  (discontinued **)
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: K-Resin® Styrene-Butadiene Copolymer (SBC)

Applications:

  • Bottles
  • Molded boxes and containers
  • Medical devices
  • Portion packages
  • Blister packaging
Features:
  • Good stiffness
  • Good formability
  • Good toughness
  • Excellent clarity with a slight blue tint
  • Enhanced mold release characteristics

Information provided by Chevron Phillips

Ineos Styrolution acquired the K-Resin® product line from Chevron Phillips Chemical Company in 2016. This grade was previously discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.01 g/ccASTM D-792
Moisture Absorption at Equilibrium 0.090 %24 hours; ASTM D-570
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 61.2ASTM D-2240
Tensile Strength, Yield 26.6 MPaType 1 @ 2.0 in/min; ASTM D-638
Elongation at Yield 236 %Type 1 @ 2.0 in/min; ASTM D-638
Flexural Strength 36.5 MPa1.0 in/min; 0.125" thickness; ASTM D-790
Flexural Modulus 1.59 GPa1.0 in/min; 0.125" thickness; ASTM D-790
Izod Impact, Notched 19.8 J/m
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D-256
Impact Test 32.8 J
@Thickness 3.17 mm,
Temperature 22.8 °C
150 in/sec; ASTM D-3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 61.1 °CASTM D-648
Vicat Softening Point 80.6 °CASTM D-1525
 
Optical PropertiesOriginal ValueComments
Gloss 148 %60°, mold temp 100°F; ASTM D-2457
Transmission, Visible 91.4 %ASTM D-1003
 
Processing PropertiesOriginal ValueComments
Mold Temperature 100 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips K-Resin® KR03NW Styrene-Butadiene Copolymer, Sheet Grade
Chemours Krytox® 103 GPL Oil
Chevron Phillips K-Resin® KR99HG Styrene-Butadiene Copolymer, Injection Molding Grade
Chevron Phillips K-Resin® KR01BR SBC
Chevron Phillips K-Resin® BK15 Styrene-Butadiene Copolymer, Injection Molding Grade

PCHEVD287 / 20781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.