MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M AC-730 Class B-2 Aerospace Sealant
Categories: Polymer; Thermoset

Material Notes: 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on aluminum and between dissimilar metals. 3M AC-730 Class B Sealants have outstanding resistance to aviation gasoline and jet fuel, as well as resistance to chemicals, hydraulic fluids and petroleum products common to the aircraft industry. The mixed compound is a thixotropic paste, easily applied by spatula, extrusion gun or injection gun. They maintain flexibility and bond strength on most metal substrates under extremes of temperature, weathering stress.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/cccured 14 days @ 50% RH
Volatiles 2.0 %
Brookfield Viscosity 950000 - 1.60e+6 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 50cured 14 days @ 50% RH
Tensile Strength at Break 2.05 MPaHeat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C
 2.07 MPaJRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C
 2.07 MPaJRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C + Heat Cycle
 2.83 MPa
@Time 1.21e+6 sec
Standard cure
 1.86 MPa
@Treatment Temp. 60.0 °C,
Time 1.04e+6 sec
JRF
Elongation at Break 60 %JRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C + Heat Cycle
 67 %Heat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C
 525 %JRF 12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C
 460 %
@Time 1.21e+6 sec
Standard cure
 390 %
@Treatment Temp. 60.0 °C,
Time 1.04e+6 sec
JRF
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °Ccured 14 days @ 50% RH
 182 °CShort term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °Ccured 14 days @ 50% RH
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
Tack-Free Time 16.0 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
 
Descriptive Properties
AppearanceBlack
 BlackAccelerator
 Off WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35402 / 170149

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.