MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Mobil Vactra 1
Categories: Fluid; Lubricant

Material Notes: The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They are formulated from high-quality base stocks and performance balanced with a progressive additive system that provides low frictional properties, excellent corrosion protection and foam resistance. A unique advanced additive package helps reduce stick-slip and chatter under thin film, boundary lubrication conditions. This allows smooth, uniform motion at design travel speeds. The Mobil Vactra Oil Numbered Series have been optimised to provide excellent separability from aqueous coolants in coolant systems while minimising the corrosive effects of high pH coolants on lubricated surfaces. The base stocks and additive package have been carefully selected to protect slides and ways while still providing good filterability. This is important because reduced flow or plugged applicator filters will increase stick-slip, chatter and wear. The metal-wetting and adhesive agents form uniform films that resist squeezing from way surfaces while the machine is not in operation.

Mobil Vactra Oil Numbered Series products are recommended both as slideway lubricants and as fluids for moderate service machine tool hydraulic systems. These oils are designed for use with all combinations of cast iron, steel and non-metallic way materials. Mobil Vactra Oil Numbered Series may be applied by hand, forced-feed lubricator or in flood application by circulation system. Their extreme pressure properties make them suitable for all types of gears found in machine tools. They should not be used in circulation systems where bulk oil temperatures exceed 66ºC. Mobil Vactra Oil No. 2 is recommended for horizontal slideways on small to medium size machine tools. It is also suitable for flood application in large machines; Mobil Vactra Oil No. 3 is recommended for dual-purpose gear and way lubrication systems; Mobil Vactra Oil No. 4 is the normal recommendation for large machines where way pressures are high or good precision is required. It is also recommended for vertical and inclined slideways where drain-down can be a problem; Mobil Vactra Oil Numbered Series can be used for lubrication of ballscrews, linear guides, headstocks, translating screws, spur and bevel gears, and lightly loaded worm gears; Applications where conventional mineral oil contamination of the aqueous coolants shortens coolant batch life

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.869 g/cc
@Temperature 15.0 °C
0.869 g/cc
@Temperature 59.0 °F
ASTM D1298
Viscosity Measurement 9696Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 31.5 cSt31.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.27 cSt5.27 cStASTM D445
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 200 kg441 lb (mass)ASTM D2783
Four Ball Wear 0.250 mm0.00984 in20 kg, 54°C, 1800 rpm, 1 hr; ASTM D4172
 
Thermal PropertiesMetricEnglishComments
Pour Point -30.0 °C-22.0 °FASTM D97
Flash Point 216 °C421 °FASTM D92
 
Descriptive Properties
Copper Strip Corrosion1B3 hrs @ 100°C
FZG 4-Square Load Support, DIN 51354, Fail Stage13
Rust Prevention, Distilled WaterpassASTM D665A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil PP7684KN Impact Copolymer
ExxonMobil PP7054L1 Polypropylene Impact Copolymer
ExxonMobil PP7033N Impact Copolymer
Braskem TI4003F Impact Copolymer Polypropylene
ExxonMobil Escorene® LD 755.12 Molding, extrusion and compounding resin

WEXXON254 / 75679

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.