Notes: Elexar® EL-3954-50 is a high performance thermoplastic elastomer designed for the electrical market. Elexar® EL-3954-50 is a lubricated, medium hardness grade suitable for both injection molding and extrusion. Features: Filled; Halogen Free; High Density; High Specific Gravity; Lubricated; Medium Flow; Medium Hardness; Slip Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Thermal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing Form: Pellets Processing Method: Extrusion; Injection Molding Information Provided by Teknor Apex |