MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Heat Resistant

Material Notes: Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDT

Features: • Bromine Free • Chlorine Free
Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219; Polyphenylene Ether + PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 1.0 - 3.0 g/10 min
@Load 11.6 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9700 psiASTM D638
Tensile Strength, Yield 10200 psiASTM D638
Elongation at Break 20 %ASTM D638
Flexural Strength 14300 psiASTM D790
Flexural Modulus 340 ksiASTM D790
Izod Impact, Notched 3.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Charpy Impact, Notched 6.00 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
Gardner Impact 200 in-lbASTM D3029
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 300 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 285 °FASTM D648
Vicat Softening Point 285 °F120°C/h, 50 N; ASTM D1525
UL RTI, Electrical 149 °F
@Thickness 1.50 mm
UL 746
 149 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 149 °F
@Thickness 1.50 mm
UL 746
 149 °F
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 149 °F
@Thickness 1.50 mm
UL 746
 149 °F
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 1.50 mm
 V-0
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 500 - 580 °F
Middle Barrel Temperature 520 - 590 °F
Front Barrel Temperature 540 - 600 °F
Melt Temperature 560 - 600 °F
Mold Temperature 180 - 240 °F
Drying Temperature 220 - 230 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.00100 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources PPX-FR5 Modified-PPO, V-0 Flame Retardant
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant

PPOLYQ214 / 160735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.