MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M 963-72 Flexible Prismatic Conspicuity Markings
Categories: Polymer

Material Notes: 3M Flexible Prismatic Conspicuity Markings Series 963 are highly retroreflective flexible microprismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detection. The reflective markings consists of prismatic lenses that are formed in a transparent, synthetic resin, reflectorized and backed with a pressure sensitive adhesive and paper liner.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 254 - 356 microns10.0 - 14.0 mil
 
Mechanical PropertiesMetricEnglishComments
Peel Strength >= 0.526 kN/m>= 3.00 pliInstron 90° pullback, 12 in/min
 
Thermal PropertiesMetricEnglishComments
Minimum Service Temperature, Air 10.0 °C50.0 °F
 
Optical PropertiesMetricEnglishComments
Gloss 100 %100 %85°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35331 / 170078

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.